When a batch of ESD POM sheet lands at a customer’s quality gate, nobody re-runs the full data sheet. Quality engineers verify a handful of values — the ones that have historically been the reason for a rejected lot. In fifteen years of watching which checks actually fire, we see the same four, over and over. Here they are, with the values that should appear on the data sheet and the standards behind them.
1. Surface resistivity: the number on the label
The headline value: carbon-filled ESD POM sits in the 10^6 to 10^9 ohms band per ASTM D257 (or IEC 62631-3-1), measured with concentric ring electrodes on a conditioned sample. This is the check that catches the wrong material — a standard POM without filler reads off-scale above 10^15 and fails instantly, and so does a sheet that has drifted. What buyers should also know: the measurement depends on conditioning. Data sheet values are given at 23 °C / 50% RH after 48 hours; a plate measured straight off the truck in a dry February warehouse can read a decade higher. Carbon-filled POM moves less with humidity than migratory grades, but it still moves. Verify at standard conditioning first; only then judge the material.
2. Volume resistivity: the check that catches the core
Surface resistivity says what a pristine face does. Volume resistivity — typically below 10^8 ohm-cm for a dissipative carbon-filled grade — says what the bulk does, and the bulk is what a machined pocket exposes. A sheet can pass the surface test while carrying an insulating skin or an inhomogeneous filler distribution, and the first milled pocket then reads like an insulator. This is the check that separates an extruded ESD compound from a surface-treated one, and it costs one extra measurement to run per ASTM D257. For any part that gets machined deeper than a few tenths of a millimetre, this value belongs in the incoming inspection, not just the data sheet.
3. Charge decay time: the functional number
Resistivity is a proxy. What the process actually cares about is how fast charge leaves: the decay from +1000 V to 100 V per ANSI/ESD STM11.31 or IEC 61340-2-3. ESD control programs built on ANSI/ESD S20.20 or IEC 61340-5-1 usually accept under 2 seconds for work surfaces and handling items; tight front-end applications want well under 1 second. A good carbon-filled ESD POM decays in fractions of a second. Why verify it when you already have resistivity? Because two materials at the same surface resistivity can decay five times apart — the decay measurement captures contact resistance and grounding path effects that the resistivity number misses, and it is the measurement your ESD coordinator will be asked about during an audit.
4. Mechanical integrity after machining: the silent failure
The fourth check is not an electrical one, and it is the one that catches the nastiest failures: does the part still have the mechanical properties the design assumed, after machining? Carbon-filled acetal retains most of the base polymer’s strength, but a few things reduce it: internal stress from wrong storage (sheets standing on edge, or stored near a heat source), machining with dull tooling that heats the surface, and moisture pickup before machining that changes dimensions and embrittlement behavior. Practical checks: dimensional stability of a machined feature re-measured after 24 hours, and a simple drop or flex test on a sample machined pocket. Typical values to hold ESD POM to: density around 1.41 g/cm³, tensile strength in the 60 MPa class, and a Rockwell M hardness around 80 — deviations well below those ranges on a certificate are a signal the material is not the grade it claims to be.
| Value | Typical target (carbon-filled ESD POM) | Standard | What it catches |
|---|---|---|---|
| Surface resistivity | 10^6 – 10^9 ohms | ASTM D257 / IEC 62631-3-1 | Wrong or drifted material |
| Volume resistivity | < 10^8 ohm-cm | ASTM D257 | Surface-only treatment, exposed core |
| Charge decay | < 2 s (1000 V to 100 V) | ANSI/ESD STM11.31 / IEC 61340-2-3 | Functional failure despite passing resistivity |
| Mechanical integrity | Density approx. 1.41 g/cm³; tensile approx. 60 MPa | ISO 1183 / ISO 527 class | Mis-stated grade, damaged stock |
How to run the four checks without slowing the dock
In practice, the four checks collapse into about an hour of work on a sample plate. Cut a ring-electrode sample and a machined test pocket from the same sheet; condition 24 to 48 hours; measure surface and volume resistivity, run the decay gun on the machined pocket, weigh a density coupon. Everything else on the data sheet — flexural modulus, heat deflection, impact values — is batch-to-batch consistency territory that the mill certificate covers. The four verified values are the ones tied to the two ways an ESD sheet actually fails in service: it stops dissipating, or it stops being the material the fixture was designed around.
Short answers
Do I need all four on every batch?For a first article and a new supplier: yes. For repeat deliveries of the same grade with mill certificates: resistivity plus decay usually suffice, with mechanical checks on first article only.
The data sheet says 10^6 – 10^9; my reading is 10^10. Reject?Check conditioning first. If the hall is dry and the plate just arrived, re-measure after 24 h at standard conditions before judging.
Which of the four fails most often?In our experience, decay time — usually from a contaminated or over-machined surface, not from the material itself.
Need a material recommendation?
Send us the application and we will reply with two or three candidate grades and a price.