Mon–Sat 08:30–18:00 (GMT+8) Founded 2009 Dongguan, China

SEMITRON grades and our equivalents: a mapping table

An RFQ that names SEMITRON grades can usually be filled from generic ESD sheet — if you know which polymer family sits behind each code. Here is the mapping we use, plus the three checks that make an equivalent stick.

ESD 6 min read
SEMITRON grades and our equivalents: a mapping table

Roughly every week an RFQ arrives that specifies SEMITRON grades by name: ESd M7 for an IC tray, ESd 225 for a wafer fixture, ESd CMP-LL for a high-humidity line. SEMITRON is a trademark of Mitsubishi Chemical Performance Polymers (originally Röchling), and the name is excellent material — but the grades sit on top of polymer families that many other producers also make. If the drawing says SEMITRON ESd M7 and nothing else, the buyer is usually paying a brand premium for a property set that a well-qualified ESD acetal matches. This note gives the mapping table we use internally, and the checks that keep an equivalent from becoming a return shipment.

The mapping table

SEMITRON grades are grouped into two families in common practice: ESd (static dissipative) and lower-resistance conductive types. The table below maps the codes we see most often to the generic family and to what we stock. Resistivity figures are typical published ranges for the family, not a guarantee for every lot — always confirm against the current data sheet.

SEMITRON grade Polymer family Generic equivalent we stock Typical surface resistivity Typical use
ESd M7 Acetal (POM), dissipative Carbon-filled ESD POM, 10^6 – 10^9 ohms 10^6 – 10^9 IC trays, electronic fixtures, machined holders
ESd M4 Acetal (POM), conductive Conductive ESD POM < 10^5 Shipping trays for charged parts, grounding paths
ESd 225 Polyetherimide (ULTEM-type), dissipative ESD PEI sheet 10^9 – 10^11 Wafer carriers, cleanroom fixtures, high-temp tooling
ESd 480 Polyetherimide, conductive Conductive PEI 10^2 – 10^5 EMI applications, conductive wafer handling
ESd CMP-LL PPS, dissipative, low moisture uptake Carbon-filled ESD PPS 10^6 – 10^9 High-humidity environments, chemical exposure, reflow-adjacent tooling
ESd 410c Polyamide-imide (PAI), conductive Conductive PAI (limited stock) < 10^5 High-temperature conductive components
ESd 520 / 500 Polybenzimidazole (PBI), dissipative / conductive ESD PBI (special order) 10^7 – 10^11 (dissipative version) Extreme-temperature handling

Two notes on reading the table. First, the numeric codes (225, 480, 410) do not encode the polymer — you have to know that 225 is PEI and 410c is PAI, which is precisely why drawings that only carry the brand code create quoting chaos. Second, ESd grades span different decades: 225 sits at 10^9 to 10^11 while M7 sits at 10^6 to 10^9, so substituting one for the other without checking the resistivity band is a specification error, not just a brand swap.

How we qualify an equivalent

When a drawing calls out a SEMITRON grade, our quotation carries a generic description plus these three checks. One: resistivity band, surface and volume, at the standard and at the actual working humidity — if the SEMITRON spec was written at 50% RH and your line runs at 25%, ask for data at both. Two: temperature and chemical exposure — a dissipative acetal cannot replace dissipative PPS in a wet, chemical environment, which is the entire point of CMP-LL; the mapping respects process conditions, not just the polymer name. Three: lot-level certification — for a requalification the buyer’s quality department will ask for a mill certificate of the ESD property, so we supply the sheet with its material certificate rather than a verbal “equivalent”.

With those three checks, the substitution succeeds in the large majority of cases. Where it fails is almost always one of two places: the buyer kept the brand name but dropped the resistivity band from the spec, and the supplier shipped something one decade off; or the part sat in a service condition (hot, wet, solvent-wiped) that the original grade was chosen to survive and the generic replacement was not.

What we need from the buyer

The fastest path is an RFQ that says: polymer family and ESD type (dissipative or conductive), resistivity band with test standard, dimensions and tolerances, service temperature and cleaning regime — and, if you like, the original brand code as a reference, clearly marked as such. We will then quote our ESD POM against ESd M7, our ESD PEI against ESd 225, our ESD PPS against ESd CMP-LL, with prices that typically run 20 to 40 percent under the branded shapes for the same property set. The brand remains yours to specify if the audit trail demands it; we stock both routes.

Short answers

Is a generic equivalent the same material as SEMITRON?It is the same polymer family with a comparable filler system; it is not the same extrusion. The property set is what you specify and test, not the brand name.

Can ESd 225 be replaced by ESD POM?Only if the temperature stays under 100 °C — 225 is a PEI with a service ceiling far above acetal. If the spec relies on that headroom, no.

Why does the brand code matter at all?Because it encodes family and resistivity in one string for people who know the table. Put the family and band in the RFQ as well, and the code becomes a convenience instead of a trap.

Need a material recommendation?

Send us the application and we will reply with two or three candidate grades and a price.

Ask an engineer
Share this article

Send us your drawing, get a price in 24 hours

Tell us the material, the size and how many pieces. If you are not sure about the material, describe the application and we will recommend one.