Two quotations arrive for an ESD sheet, one specified at 10^6 to 10^8 ohms and one at 10^9 to 10^11, and the buyer asks whether the cheaper one is equivalent because both are “static dissipative”. It is not, and the difference is not a matter of degree — it changes what the material can protect, how it behaves in dry air, and whether it survives cleaning. This note explains what the resistivity number actually controls.
Surface or volume: the first thing to pin down
Most data sheets quote surface resistivity in ohms per square, measured per ASTM D257 or IEC 62631-3-1 with a concentric ring electrode. That is the right number for a worksurface, a tray or a tote, because the charge you are draining sits on the surface. For a machined part — a fixture, a wafer boat, a component holder — the relevant quantity may be volume resistivity in ohm-centimetres, because the grounding path runs through the material, not along it. A sheet can be surface-dissipative while its core is far more insulating, and a machined pocket can expose that core.
When you write a specification, name both: surface resistivity range, volume resistivity range, the test standard, and the conditioning before test. A supplier who only quotes one number has told you half the story.
What the decades mean in practice
| Surface resistivity | Class | Behaviour | Typical use |
|---|---|---|---|
| < 10^5 | Conductive | Near-metal; fast decay; spark risk if a charged device touches it | IC trays for shipping, grounding paths, EMI housings |
| 10^6 – 10^8 | Dissipative, tight | Fast decay (well under 2 s), controlled discharge | Bare device handling, hard drive assembly, Class 0 HBM |
| 10^9 – 10^11 | Dissipative, loose | Slower decay (seconds), sensitive to humidity and wear | Bench tops, storage bins, general electronics assembly |
| > 10^12 | Insulating | Charge persists; not ESD-safe | Not acceptable in an ESD area |
The 10^6 to 10^8 band exists for one reason: a device that is already charged must not be discharged so fast that the current pulse damages it. Below 10^5, contact with a charged board produces a current spike that a thin gate oxide cannot survive. Between 10^6 and 10^8 the discharge is fast enough to prevent charge accumulation and slow enough to limit peak current — which is why semiconductor front-end and disk drive lines specify the tighter band, and why a 10^9 sheet is not accepted there even though both are “dissipative”.
Humidity: the hidden variable
Antistatic grades that rely on migratory additives depend on moisture to work. At 50 percent relative humidity they may sit at 10^9; in a dry room at 12 percent RH the same sheet can drift to 10^11 or 10^12 and stop protecting anything. Carbon-loaded grades shift far less, typically within one decade across the humidity range. If your process includes a dry room, a cleanroom with low humidity, or winter air in an unhumidified plant, this is the variable that will bite — and it is exactly the variable a data sheet measured at 23 °C / 50 percent RH does not show you.
Ask for resistivity at two humidities, or for the charge decay time at the humidity you actually run. A supplier who cannot provide either is selling a room-condition number.
Charge decay is the property that matters
Resistivity is a proxy. The functional property is how fast a charge dissipates, measured as decay time from 1000 V to 100 V (or per IEC 61340-2-3 / ANSI/ESD STM11.31). For worksurfaces and handling equipment in an ESD control program to IEC 61340-5-1 or ANSI/ESD S20.20, decay under 2 seconds is the usual acceptance line; tight-front-end applications often demand well under 1 second. Two materials with the same surface resistivity can differ in decay time by a factor of five, because resistivity measures a steady-state property while decay measures the dynamic path — including contact resistance to the ground point, which is where most real installations fail.
Degradation: how ESD sheets lose their property
Three mechanisms, in order of frequency. First, cleaning: migratory antistatic additives sit at the surface and are wiped away by aggressive solvents or abrasive pads, taking the dissipative property with them. Second, abrasion: a machined or worn surface exposes fresh material that may have a different filler concentration, and carbon-loaded grades can develop insulating smears from machining coolant residue. Third, contamination: hydrocarbon oils and silicone sprays form an insulating film over a perfectly good sheet.
Specify a cleaning agent that is compatible, verify decay time after cleaning rather than only on delivery, and re-test periodically. An ESD program that tests the sheet once at goods-in and never again is measuring the wrong thing.
Writing a specification that holds
A workable ESD callout reads like this: material and grade; surface resistivity 10^6 to 10^8 ohms per ASTM D257, conditioned 48 h at 23 °C / 50 percent RH; volume resistivity below 10^6 ohm-cm; charge decay from 1000 V to 100 V under 2 s at the same conditioning; cleaning agent compatibility statement; batch test certificate. Add the application class — bare device, loaded board, or enclosed assembly — because that is what determines whether the tight band is required.
Questions from ESD audits
Can I use a 10^9 sheet on a bare device line? Only if your ESD control plan and the device sensitivity analysis say so. Most Class 0 and Class 1 HBM lines specify the tighter band for a reason.
Is black always conductive? No. Black usually means carbon black, which is often conductive, but black pigment alone proves nothing. Ask for the number.
Does thickness change resistivity? Surface resistivity is nominally independent of thickness; volume resistivity is not, and through-thickness resistance scales with thickness. For machined parts, specify which one you mean.
Why does my sheet fail in winter? Dry air. Either move to a carbon-loaded grade or add humidity control; testing at 12 percent RH will show it immediately.
Need a material recommendation?
Send us the application and we will reply with two or three candidate grades and a price.