PEEK sheet thickness range: what actually ships from stock

Every distributor quotes a PEEK sheet thickness range. Only part of it is a stock item, and the rest behaves differently in tolerance, lead time and price.

Material Selection
PEEK sheet thickness range: what actually ships from stock

Ask three suppliers for a PEEK sheet and you will get three different answers about thickness. One quotes 0.5 mm to 100 mm as if the whole band were one product. A second offers 6 mm to 40 mm and calls everything else made to order. A third asks for a drawing before answering at all. None of them is wrong. The range is real, but it is not uniform: below roughly 4 mm and above roughly 50 mm the material changes how it is manufactured, and that changes tolerance, price and lead time.

This page is about the part of the question buyers actually need answered: which thicknesses can be shipped this week, which ones carry a machining allowance, and where the numbers in a quotation come from.

One thickness range, three different products

PEEK sheet in the market is made by three routes, and each route owns a band of thickness.

  • Extruded sheet. Pellets are melted and pushed through a die, then run through a calender and a cooling line. This is the workhorse for 4 mm to about 50 mm. It gives the most consistent surface, the lowest internal stress and the best machining behaviour, which is why almost every stocked sheet is extruded.
  • Compression moulded block. Powder is sintered and pressed in a heated mould. Above about 50 mm, extrusion becomes slow and expensive, so thick block is moulded instead. Moulded block is denser in the core but carries more residual stress, and it has to be annealed before it is machined into a part that must stay flat.
  • Skived sheet and film. A thick billet is rotated against a blade and peeled into thin sheet. This is how very thin PEEK is produced. Thickness control is good, flatness is not: skived sheet shows a slight curl and needs flattening or fixture support during machining.

A quotation that treats all three as the same product will be wrong on at least two of them.

The four bands, and what each one is good for

Thickness band How it is made Stock situation What to watch
0.5 to 3 mm Skived or extruded film Usually made to order Flatness, minimum order quantity, edge quality
4 to 12 mm Extruded sheet Normally stocked, cut to size Tolerance class, annealing before machining
15 to 40 mm Extruded sheet Normally stocked Machining allowance, stress relief
45 to 100 mm Moulded block or heavy extrusion Made to order, two to four weeks Core voids, annealing, saw loss on the cut

The practical reading of that table: if your part is between 6 mm and 40 mm, you are buying from a shelf and the only variables are tolerance and cutting. Outside that band you are buying a production run, and the supplier needs a quantity before the price means anything.

Tolerance is where thickness stops being a number

A nominal 20 mm sheet is not 20.000 mm. Thermoplastic sheet is supplied against tolerance tables such as EN 15860 or the older DIN 16985, and the allowance widens as the sheet gets thicker, because the material shrinks as it cools and the shrink is not identical across a wide web.

In practice the numbers look like this: a 6 mm extruded sheet typically holds plus or minus 0.2 to 0.4 mm; a 30 mm sheet typically holds plus or minus 0.5 to 1.0 mm; a 60 mm moulded block can be plus or minus 1.5 mm or more. If the drawing asks for 20 mm plus or minus 0.05 mm, you are not buying sheet, you are buying a ground sheet, and that is a different line item: grinding removes material on both faces, adds a day or two, and usually adds 15 to 25 percent to the piece price.

Two habits save arguments later. First, specify the tolerance you need for the finished part, not for the raw sheet, and let the supplier decide whether that means a thicker starting stock. Second, if the part is a seal seat or a locating face, ask for the flatness figure, not just the thickness. A 20 mm sheet inside tolerance can still be bowed by 0.3 mm across a 500 mm length.

Thickness changes the material, not just the dimensions

This is the part that surprises engineers who are used to metals. In PEEK, the cooling rate through the thickness decides how crystalline the polymer becomes, and crystallinity decides how the part behaves in service.

  • Crystallinity. Slow cooling gives a more crystalline sheet: stiffer, more wear resistant, more dimensionally stable at temperature, and slightly more brittle. Fast cooling gives a tougher but less stable sheet. Thin sheet cools fast, thick block cools slowly, so a 3 mm sheet and a 60 mm block are not the same material in service even when both are unfilled PEEK.
  • Residual stress. Thick extruded and moulded stock carries stress from the cooling gradient. Machine a pocket into it and the stress releases, and the part moves. The fix is an anneal before finish machining, typically just below the glass transition temperature, held long enough for the core to catch up, then cooled slowly.
  • Skin and core. In moulded block the outer skin is denser than the core. If you machine a deep pocket, you may expose slightly more porous material. For vacuum service or for sealing faces, keep the machined surface in the outer third of the block, or specify a void-free grade.

Matching the thickness to the job

The thickness usually comes from the application rather than from the drawing.

  • Seal rings and backup rings, 1 to 3 mm. Thin, tight tolerance, no voids. Here you want skived or thin extruded sheet and a flatness requirement written into the purchase order.
  • Wear pads and guide strips, 6 to 20 mm. Thickness matters less than the filler system. Glass filled and carbon filled grades buy wear resistance at the cost of mating-surface wear.
  • Wafer handling and ESD fixtures, 8 to 20 mm. Flatness and cleanliness dominate. The sheet must be annealed, and it should be machined in a way that does not embed contamination in the surface.
  • Bushings, rollers and seals in profile, 20 mm and up. These are usually cut from rod, not sheet. A sheet has a grain direction from the extrusion and a rod does not, so a bushing machined from sheet can wear unevenly around its circumference.

That last point is worth repeating because it is a common and expensive mistake: sheet and rod are not interchangeable starting stock. If the part is rotationally loaded, start from rod even when the sheet is cheaper per kilo.

What to put on the RFQ

A PEEK sheet enquiry that answers these six points comes back with a usable price the same day. One that does not usually comes back with a question.

  1. Nominal thickness and the tolerance you need on the finished part.
  2. Quantity, stated both in sheets and in finished pieces, plus the cut pattern if there is one.
  3. Whether the grade is unfilled, glass filled, carbon filled or bearing grade, and whether a brand equivalent is acceptable.
  4. Flatness or parallelism if the part is a sealing or locating surface.
  5. Whether the material must be annealed, and whether the supplier or your shop does it.
  6. Documentation: certificate of analysis, lot traceability, and any food contact or biocompatibility statement.

Adding a drawing to those six answers removes most of the remaining ambiguity, even for a simple rectangular part.

How we hold PEEK sheet

Top Plastic stocks PEEK sheet in the machining bands where customers order most often, and cuts to size on a panel saw so a buyer is not forced to take a full 1000 by 2000 mm sheet for a 300 mm part. Thicknesses outside the stocked band are quoted against the next production run, with the lead time stated up front rather than discovered after the order.

If you are choosing between two thicknesses, or between sheet and rod, send the drawing and the load case. The answer usually takes less time than a trial cut. Details of the grades we hold are on the PEEK material page, and semiconductor applications are covered in the semiconductor industry guide.

Need a material recommendation?

Send us the application and we will reply with two or three candidate grades and a price.

Ask an engineer
Share this article

Send us your drawing, get a price in 24 hours

Tell us the material, the size and how many pieces. If you are not sure about the material, describe the application and we will recommend one.

Request a quote Browse stock shapes