ERTALYTE TX (PET-P) for precision parts: where it beats acetal

PET-P costs more per kilogram than acetal and buys it back in dimensional stability. The places it pays: humid shops, 80 to 100 C service, low-creep fixtures, and dry sliding against steel.

Material Selection 8 min read
ERTALYTE TX (PET-P) for precision parts: where it beats acetal

On most machining quotations, extruded PET-P under a brand like ERTALYTE TX sits visibly above acetal in price. Buyers who only compare modulus and strength reject it, because the numbers look close: both are around 2.9 to 3 GPa in modulus, both machine cleanly, both stock well. The price gap is not explained by the data sheet’s first page — it is explained by what happens to each material after it leaves your shop and spends a year in the customer’s environment. This note sets out the cases where the PET-P premium is money well spent, and the two cases where acetal is still the better answer.

The moisture number that decides precision

The decisive difference is water. Acetal (POM-C) absorbs roughly 0.8 percent water at saturation in 50 percent relative humidity, and a machined dimension moves visibly as it equilibrates. Extruded PET-P absorbs roughly a quarter to a third of that — typical data sheets list 0.2 to 0.3 percent at 50 percent RH — and the corresponding dimensional movement is smaller by the same order. For a 100 mm dimension, that is the difference between a part that drifts by tenths of a millimetre over its first humid season and one that stays inside a ±0.1 mm window.

This is why PET-P shows up repeatedly in exactly the parts where acetal disappoints: guide blocks and fixtures that hold position across a humid summer, optical and measurement equipment holders where a drifted datum ruins calibration, and components installed in washdown environments where daily hot water cycles keep pushing acetal parts toward their saturation value. If your tolerance budget is tight and your environment is wet, the PET-P premium is cheaper than the first rework round.

Stiffness and creep at operating temperature

At room temperature the two materials are genuinely close, and neither wins on stiffness. Above roughly 70 °C the picture changes, because PET-P has a glass transition near 76 °C and a melting point near 250 °C, while acetal copolymer softens from a crystalline melting range around 165 °C with no reinforcing transition to lean on. In practical terms:

  • 80 to 100 °C continuous service: PET-P retains useful stiffness and threaded features hold preload visibly better than POM-C, which relaxes and creeps under sustained load in this range.
  • Low-creep fixtures: clamping elements, locating pads and press-fit sleeves that must not relax over months perform measurably better in PET-P.
  • Short thermal excursions: PET-P tolerates brief exposure well above 100 °C without permanent deformation; acetal takes a permanent set.

None of this makes PET-P a high-temperature material in the PEEK sense — 100 °C continuous is the honest ceiling — but within the band where acetal starts to lose its nerve, PET-P keeps its shape.

Dry sliding against steel

ERTALYTE TX is the sliding-enhanced grade: solid lubricant dispersed through the PET-P matrix feeds the running surface as the material wears. Against steel, in unlubricated service, it runs a lower friction coefficient and longer wear life than natural PET-P, and it does so with the low moisture uptake already described — which matters, because a sliding element that swells with humidity changes its own running clearance. Typical TX applications: wear pads, conveyor guides, wiper blades, sliding bushings in equipment that runs dry.

Against gears specifically, be careful before converting: acetal gears remain the better choice at fine modules because of toughness and machinability of small features, and PET-P does not out-slip MC901 nylon in dry heavy-load service. TX wins in the middle ground — moderate loads, dry running, and dimensional clearance that must survive humidity.

Side-by-side

Property / condition PET-P (TX sliding grade) Acetal POM-C
Moisture at 50 % RH saturation 0.2–0.3 % 0.8 %
Dimensional drift, 100 mm part Minor, stays in tight windows Tenths of mm across seasons
Stiffness at 80–100 °C Useful retention, low creep Relaxes under sustained load
Dry friction against steel Low (TX), stable over time Low, better impact toughness
Machining small fine features Good Excellent
Price per kg, extruded rod Higher Lower
Chemical weak spot Strong alkalis Strong acids

That last row deserves a sentence: PET-P resists mineral acids that slowly attack acetal, while strong alkalis attack PET the way acids attack POM. Match the chemistry of the washdown or process fluid before the choice is finalized.

Where acetal still wins

Two honest cases. First, price-governed precision: if the environment is dry, the temperature never passes 60 °C and the tolerance is achievable in POM-C, paying the PET-P premium buys stability you will not use. Second, small intricate features: acetal machines crisper edges and finer threads with less tool wear chatter, and its slightly better toughness protects thin sections during assembly. A precision acetal part in a dry, cool environment is not a compromise — it is the correct material.

Equivalent brands if TX is unavailable

The TX-type sliding PET-P grade appears under several names: TECAPET TX from Ensinger is the closest cross-reference, and the natural PET-P grades ERTALYTE and TECAPET natural serve the non-sliding duty. Ask suppliers to confirm the grade is extruded PET-P, request the moisture and creep data rather than the headline tensile values, and if the part is a sliding element, insist on the internally lubricated version — natural PET-P in a dry sliding application wears several times faster.

Questions we answer weekly

Is PET-P harder to machine than acetal? Marginally. It cuts cleanly with sharp carbide, produces less gummy chips than nylon, but needs sharper tooling than POM for mirror finishes. For tolerance-critical features, machine PET-P dry and let it rest before final passes — its low moisture uptake means almost no post-machining drift, which is the point of the material.

Can I replace an existing POM part with PET-P without redesign? Usually yes where the driver was dimensional drift or heat relaxation. Check press-fits first: PET-P’s slightly different modulus and thermal expansion shifts interference fits by small amounts — verify critical fits at both temperature extremes.

Is the price gap stable? PET-P stock shapes are produced in smaller volumes than POM, so quotes fluctuate more. For repeat programs, agree a frame price for the year rather than buying per order.

Need a material recommendation?

Send us the application and we will reply with two or three candidate grades and a price.

Ask an engineer
Share this article

Send us your drawing, get a price in 24 hours

Tell us the material, the size and how many pieces. If you are not sure about the material, describe the application and we will recommend one.

Request a quote Browse stock shapes