Mon–Sat 08:30–18:00 (GMT+8) Founded 2009 Dongguan, China

Why we anneal PEEK before machining, and what happens if you skip it

Extruded PEEK carries locked-in stress from the extrusion process. Machine it out and the part will move. One controlled heating cycle removes the problem.

Machining 6 min read
Why we anneal PEEK before machining, and what happens if you skip it

PEEK arrives from the extruder with residual stress locked into it. The material was pushed through a die at over 350 C and cooled under tension, and that history stays in the sheet or rod until something releases it.

Machining is what releases it. Cutting removes material from one side of a plate, which unbalances the internal stress and lets the part bow. The effect is small on a 10 mm plate and dramatic on a 60 mm one — a few tenths of a millimetre of bow is normal, and on a seal face a few tenths is a leak.

The fix is an annealing cycle: heat the stock or the roughed-out part to a defined temperature below the melting point, hold it long enough for stress to relax, then cool slowly and in a controlled way. We anneal stock above 25 mm before machining and rough-machine then anneal again for parts with tight flatness requirements. Cooling rate matters as much as hold time — a fast cool puts new stress back in. If you are buying PEEK and machining it yourself, ask us to supply pre-annealed stock.

Need a material recommendation?

Send us the application and we will reply with two or three candidate grades and a price.

Ask an engineer
Share this article

Send us your drawing, get a price in 24 hours

Tell us the material, the size and how many pieces. If you are not sure about the material, describe the application and we will recommend one.

Request a quote Browse stock shapes