PTFE Virgin Sheet, Rod and Tube
Lowest friction of any solid, −200 °C to +260 °C, universal chemical resistance.
Glass-filled PTFE with 4× better wear resistance and reduced creep under load.
PTFE sheet, rod and tube are supplied in virgin and filled grades. Glass-filled PTFE improves wear and creep; graphite-filled PTFE adds thermal conductivity and electrical conductivity. Used for gaskets, seals, linings and electrical insulators.
| Material family | PTFE — Polytetrafluoroethylene |
|---|---|
| Stock form | Sheet and Rod |
| Colour | White / grey |
| Continuous service temperature | 260 °C |
| Available sizes | Sheet 3–50 mm · Rod Ø10–150 mm |
| Temperature class | Advanced Engineering |
Values are typical for the unfilled grade and are given for guidance. Request the current lot certificate for specification purposes.
| Density | 2.16 g/cm³ |
|---|---|
| Tensile strength | 25 MPa |
| Continuous service temp. | 260 °C |
| Coefficient of friction | 0.05 – 0.10 |
| Water absorption (24 h) | Below 0.01 % |
| Dielectric constant | 2.1 |
Send the plate size or rod length and diameter. Saw cut and squared within 48 hours of order confirmation.
Send DXF, STEP or a dimensioned PDF. Milled, turned and faced to your tolerance, inspection report on request.
Certificate of conformity with grade, colour and lot number. FDA, EU 10/2011 and ISO 10993 paperwork where the grade supports it.
Moisture barrier, edge protection and wooden case. Air, LCL and FCL shipping with full export documentation.
Lowest friction of any solid, −200 °C to +260 °C, universal chemical resistance.
Unfilled virgin PEEK — the highest specification stock shape we hold, machinable to ±0.02 mm.
Carbon-fibre reinforced PEEK with 3× the stiffness and 2× the thermal conductivity of unfilled PEEK.
Tell us the material, the size and how many pieces. If you are not sure about the material, describe the application and we will recommend one.